Posted by Jon Elson
on 2008-04-02 09:42:55 UTC
Yahoo wrote:
> Where in the heck does one get molybdenum disulfide and PTFE in powder form?
I've got several pounds of "virgin Teflon", ie. the stuff as it
is scraped out of the pressure vessels where it is formed. it
looks something like snow with powdered sugar mixed in. If
anyone needs some, I am not using it. (It is used in this form
to fill molds, but my mold had too complex a shape and I got
uneven filling, so I ended up having to machine the parts from
solid. So, I have lots left over.)

Molybdenum diSulfide is usually added into a grease, and for the
epoxy project you need the non-greased stuff. I suspect it will
be harder to find in that form.

Jon

Discussion Thread

Yahoo 2008-04-02 07:31:56 UTC Re: "Homemade moglice" Jon Elson 2008-04-02 09:42:55 UTC Re: [CAD_CAM_EDM_DRO] Re: "Homemade moglice" Ralph Reese 2008-04-02 09:53:24 UTC RE: [CAD_CAM_EDM_DRO] Re: "Homemade moglice" Peter Reilley 2008-04-02 10:22:57 UTC Re: [CAD_CAM_EDM_DRO] Re: "Homemade moglice" H & J Johnson 2008-04-02 12:11:29 UTC Re: [CAD_CAM_EDM_DRO] Re: "Homemade moglice" jesse Brennan 2008-04-02 12:45:29 UTC Re: [CAD_CAM_EDM_DRO] Re: "Homemade moglice" turbulatordude 2008-04-02 12:46:28 UTC Re: "Homemade moglice" Yahoo 2008-04-02 13:02:40 UTC Re: "Homemade moglice" Graham Stabler 2008-04-06 10:43:56 UTC Re: "Homemade moglice" turbulatordude 2008-04-06 11:11:33 UTC Re: "Homemade moglice" Jim Register 2008-04-06 17:33:13 UTC Re: "Homemade moglice"