For plexiglas try your local glass shop. They will certainly stock 1/4" but may have to order thicker stuff.
A person that is careful with a torch..(smoky C2H2 flame, i.e. cool ) can polish cut or machined edges. A light touch is
necessary...your milage may vary.
Good Luck, sounds like a neat project.
Dave
A person that is careful with a torch..(smoky C2H2 flame, i.e. cool ) can polish cut or machined edges. A light touch is
necessary...your milage may vary.
Good Luck, sounds like a neat project.
Dave
Discussion Thread
Michael McLaughlin
2000-10-02 21:41:25 UTC
Milling Materials
Dan Dowell
2000-10-02 21:45:53 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
Alan Marconett KM6VV
2000-10-02 23:06:54 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
Michael McLaughlin
2000-10-03 05:34:28 UTC
RE: [CAD_CAM_EDM_DRO] Milling Materials
Rick Dulas
2000-10-03 06:18:55 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
Dan Mauch
2000-10-03 07:27:07 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
dave engvall
2000-10-03 07:58:52 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
Alan Marconett KM6VV
2000-10-03 10:40:26 UTC
Re: [CAD_CAM_EDM_DRO] Milling Materials
Bill
2000-10-03 14:35:41 UTC
RE: Milling Materials
scott3d3@a...
2000-10-24 17:10:13 UTC
Re: Milling Materials
Smoke
2000-10-24 20:18:40 UTC
Re: [CAD_CAM_EDM_DRO] Re: Milling Materials
Jon Elson
2000-10-24 22:35:27 UTC
Re: [CAD_CAM_EDM_DRO] Re: Milling Materials
Anne Ogborn
2000-10-25 09:29:08 UTC
Re: [CAD_CAM_EDM_DRO] Re: Milling Materials