What are you molding? What kind of resin? The reason that I ask is
that we do a lot of carbon fiber reinforced polymer conmposite molding
at work. (We develop high-temperature resins)
If you use either cloth or continuous fiber you can make strong,
lightweight parts that are really stiff - which might be just the
thing for some of these home made routers so many people are working on.
Chris
that we do a lot of carbon fiber reinforced polymer conmposite molding
at work. (We develop high-temperature resins)
If you use either cloth or continuous fiber you can make strong,
lightweight parts that are really stiff - which might be just the
thing for some of these home made routers so many people are working on.
Chris
Discussion Thread
tom sommerville
2003-09-04 14:41:16 UTC
Home brew nuts: squeezing of, in vise-- Release Agent
Graham Stabler
2003-09-04 16:39:34 UTC
Re: Home brew nuts: squeezing of, in vise-- Release Agent
jchrisj7734
2003-09-07 12:07:02 UTC
Re: Home brew nuts: squeezing of, in vise-- Release Agent
jpfalt
2003-09-07 12:07:08 UTC
Re: Home brew nuts: squeezing of, in vise-- Release Agent
turbulatordude
2003-09-07 14:52:17 UTC
Re: Home brew nuts: squeezing of, in vise-- Release Agent