CAD CAM EDM DRO - Yahoo Group Archive

RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier

Posted by Jack Hudler
on 2006-03-02 17:35:43 UTC
(Hit send by accident)
I'm actively searching for a supplier


http://www.chockfastgrout.com/industrial/index_indust.html

See ChockFast Red Technical Bulletins #559 and 617Q. Looks like this stuff can
pour up to 18 inches so this stuff will be great for filling columns. I don't
think you need to worry about the 18 inch limit on columns, due to there small
diameters I don't believe runaway or excessive exothermic reaction causing poor
cure will happen.
However, this stuff is perfect for filling machine bases.

Here's the marketing language;

CHOCKFAST RED is a user-friendly, chemically resistant, low dusting epoxy grout
with high compressive, tensile and shear strengths. Excellent compatibility with
concrete and steel minimizes or eliminates horizontal bond-line cracks, common
to traditional epoxy grouts. This 24-hr cure structural epoxy is formulated to
provide *excellent vibration damping* for static and dynamic loads plus
permanent monolithic support with intimate contact between equipment bedplates
and underlying concrete foundations. A gentle exothermic reaction during cure
reduces cast-in stresses and allows single pours up to 18". (For single pours
deeper then 18", contact a CHOCKFAST Representative.) Deep pours expedite
installation of new equipment. They also reduce costly downtime for foundation
repairs. Low dusting formulation simplifies installation and cleanup procedures.
Tools and mortar mixers can be cleaned with water.

Discussion Thread

Elliot Burke 2006-02-28 11:31:02 UTC re:RE: re:RE: Epoxy Granite, SPDT glass Jon Elson 2006-02-28 18:31:33 UTC Re: [CAD_CAM_EDM_DRO] re:RE: re:RE: Epoxy Granite, SPDT glass wanliker@a... 2006-02-28 19:15:18 UTC RE: Epoxy Granite, SPDT glass yahoo@h... 2006-02-28 20:00:19 UTC Re: [CAD_CAM_EDM_DRO] RE: Epoxy Granite, SPDT glass yahoo@h... 2006-02-28 20:12:02 UTC Re: [CAD_CAM_EDM_DRO] re:RE: re:RE: Epoxy Granite, SPDT glass Graham Stabler 2006-03-01 03:59:51 UTC Re: Epoxy Granite, SPDT glass Jack Hudler 2006-03-01 07:00:07 UTC RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite, SPDT glass Graham Stabler 2006-03-01 11:40:25 UTC Re: Epoxy Granite, SPDT glass wanliker@a... 2006-03-01 12:14:01 UTC Re: Epoxy Granite, SPDT glass john_glynn57 2006-03-01 14:56:04 UTC Re: Epoxy Granite, SPDT glass Graham Stabler 2006-03-02 07:36:29 UTC Re: Epoxy Granite supplier Dan Tyler 2006-03-02 08:27:40 UTC Re: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Graham Stabler 2006-03-02 14:37:33 UTC Re: Epoxy Granite supplier Jack Hudler 2006-03-02 17:20:03 UTC RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Jack Hudler 2006-03-02 17:35:43 UTC RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Harko Schwartz 2006-03-05 07:32:49 UTC Re: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Jack Hudler 2006-03-06 01:12:11 UTC RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Harko Schwartz 2006-03-06 09:10:30 UTC Re: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Jack Hudler 2006-03-06 17:35:17 UTC RE: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier Harko Schwartz 2006-03-06 18:12:00 UTC Re: [CAD_CAM_EDM_DRO] Re: Epoxy Granite supplier