CAD CAM EDM DRO - Yahoo Group Archive

Re: [CAD_CAM_EDM_DRO] Moglice ?

Posted by ptengin@a...
on 2000-05-17 10:27:00 UTC
In a message dated 05/17/2000 3:40:37 AM Hawaiian Standard Time,
dmauch@... writes:

<< It would be
interesting to mix some of the cheaper expoxies with anti seize to9 see if
it will cure properly
Dan >>
Dan,

If solvent was used to wash out the oil in "anti seize" and only the dry
powder portion is mixed into the epoxy, I bet good results could be obtained.
Put some anti seize in a large glass jar and add acetone or some other good
solvent. Shake well and decant the next morning. Do this a couple of times
and you should get most if not all of the oil out of the mixture. I did this
to buffing compound bars to obtain the "grit" also.
FYI

Peter
THRD, Inc.

Discussion Thread

Ron Ginger 2000-05-16 12:17:21 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? Jon Anderson 2000-05-16 12:31:33 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? Ron Ginger 2000-05-16 13:07:54 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? Tim Goldstein 2000-05-16 14:11:27 UTC RE: [CAD_CAM_EDM_DRO] Moglice ? Steve Carlisle 2000-05-16 20:07:36 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? Dan Mauch 2000-05-17 06:39:30 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? ptengin@a... 2000-05-17 10:27:00 UTC Re: [CAD_CAM_EDM_DRO] Moglice ? Paul Devey 2000-05-17 13:47:16 UTC RE: [CAD_CAM_EDM_DRO] Moglice ?